Tianjin Zhongyuanyuanda Steel Co.,Ltd.
|
Payment Terms: | T/T,L/C |
Place of Origin: | Shanghai, China (Mainland) |
![]() |
|
Add to My Favorites | |
HiSupplier Escrow |
Specifications | |
Material | Type 316L SS Sheets/sheet/PLATES/plate |
Shapeform | Coil |
Preparation | Paper Interleaved Vinyl Masked |
Thickness | 20 gauge |
Thickness | 0.0355 inches |
Size | 30*Coil |
Width | 30 |
Sheet Weight Per Unit Area | 1.512 lbs/ft² |
Finish | No.2B No.3 No.4 |
Condition | Cold Rolled Annealed |
Nominal Composition | 0 to 0.25% Carbon 1.00% Max. Silicon 2.00% Max. Manganese 6 to 36% Nickel 7 to 30% Chrome |
ASM Specification | ASTM A240 ASTM A262 Prac E ASTM A480 ASTM SA-240 UNS S31603 |
Typical Mechanical Properties | |
Steel Alloy Group | Austenitic |
Magnetic Properties | Non-Magnetic |
Harden By | Cold Work |
Corrosion Resistance | High |
Hardness | Low to Med. |
Strength | Low to Med. |
Ductility | High |
Toughness | High |
Elec.Conductance | Low |
Thermal Conductance | Low |
Thermal Expansion | High |
Heat Resistance(Scaling Strength) | High |
Comparative Characteristics and Applications | |
Yield Strength | 45000 lbs/in² |
Tensile Strength | 18200 lbs/in² |
Elongation percent in 2 inches | 50% |
Hardness (Rockwell B) | 83 |
Creep Strength Load for 10000 Hr.with 1% Elongation at 1000°F | 25000 lbs/in² |
Creep Strength Load for 10000Hr.with 1% Elongation at 1100°F | 7900 lbs/in² |
Creep Strength Load for 10000Hr.with 1% Elongation at 1200°F | 7900 lbs/in² |
Creep Strength Load for 10000Hr.with 1% Elongation at 1300°F | 7900 lbs/in² |
Density | 0.29lbs/in² |
Modulus of Elasticity in Tension | 29.0 x 106 lbs/in² |
Specific Heat (32 to 212°F) | 0.12 BTU/ºF/lbs |
Thermal Conductivity at 212°F | 9.04 BTU/hr.ft²/ft/ºF |
Thermal Conductivity at 932°F | 12.4 BTU/hr.ft²/ft/ºF |
Mean Coefficient of Thermal Expansion per°F(32 to 212°F) | 8.8 x 10-6 ºF |
Mean Coefficient of Thermal Expansion per°F(32 to 600°F) | 9.0 x 10-6 ºF |
Mean Coefficient of Thermal Expansion per°F(32 to 1000°F) | 9.7 x 10-6 ºF |
Mean Coefficient of Thermal Expansion per°F(32 to 1200°F) | 10.3 x 10-6 ºF |
Melting Point Range | 2500 to 2550 ºF |
Electrical Resistivity | 74 µΩ.cm |
Max.Operating Temp.(Continuous Service) | 1700 ºF |
Max.Operating Temp.(Intermittent Service) | 1600 ºF |
Welding Properties | Good |
Drawing and Stamping | Good |
Hot Working-Initial Forging | 2100 to 2300 ºF |
Annealing Temp. | 1950 to 2050 ºF |
Stress Relieving Temp. | 400 to 750 ºF |